ZG230-450 Material Data
ZG230-450 Element content C:≤0.30 Si:≤0.50 Mn:≤0.90 P:≤0.04 S:≤0.04 Heat treatment Normalizing or annealing temperature:890-910℃ Tempering temperature:620-680℃ Mechanical properties Tensile strength:450MPa Yield strength:230MPa Elongation:22% Section shrinkage:32% Impact:25J The ZG230-450 material characteristics: low-carbon cast steel , strength and low hardness , toughness and good plasticity , high low temperature impact toughness , low- brittle transition temperature , electrical conductivit...
ZG200-400 Material Data
ZG200-400 Element content C:≤0.20 Si:≤0.50 Mn:≤0.80 P:≤0.04 S:≤0.04 Heat treatment Normalizing or annealing temperature:920-940℃ Mechanical properties Tensile strength:400MPa Yield strength:200MPa Elongation:25% Section shrinkage:40% Impact:30J The ZG200-400 material characteristics: low-carbon cast steel , strength and low hardness , toughness and good plasticity , high low temperature impact toughness , low- brittle transition temperature , electrical conductivity, electromagnetic properties o...